Austenitic stainless steel stabilized with Ti, used similarly as V304L.
- ABTN | ASTM | SAE | AISI: 321
- DIN | WNr: 1.4541
- Chemical composition:
C % | Mn % | Cr % | Ni % | Mo % | W % | Si % | OTHERS % |
max. 0.08 | max. 2.00 | 18.00 | 10.50 | - | - | <=1.00 | Ti<=0.70 |
Austenitic stainless steel stabilized with Ti, used similarly as V304L.
C % | Mn % | Cr % | Ni % | Mo % | W % | Si % | OTHERS % |
max. 0.08 | max. 2.00 | 18.00 | 10.50 | - | - | <=1.00 | Ti<=0.70 |